In this study the durability of high alumina cement (HAC) with different composition of clinkers, in terms of resistance of chloride transport, was evaluated. The composition of clinkers in HAC were determined by quantitative X-ray analysis (Q-XRD) using Rietveld method. For a development of the strength, the penetration resistance of fresh mortar was immediately measured after mixing at a given time interval and the compressive strength of mortars cured in a wet chamber at 25±2 °C was measured at 1-91 days. To assess the risk of corrosion of steel in specimen, the diffusion cell test was performed and simultaneously a further experimentation including an examination of the pore structure, chloride binding was carried out. As a results, it was found that an increase in CA clinker content resulted in an increase in the setting time, which affected the development of the strength; maximum strength for Union 50 was much higher, and then continuously reduced until 91 days due to conversion. For the rate of chloride transport, however, the lower effective coefficient of diffusion was obtained in Union 50, arising from poor pore connectivity in the cement matrix after conversion process. © 2018 by Korea Concrete Institute.
키워드
- 제목
- 알루미나 시멘트 내 클링커 조성에 따른 염소이온 침투 저항성 평가
- 제목 (타언어)
- Evaluation of rate of chloride transport for alumina cement mortar with different composition of clinkers
- 저자
- 양희준; 심현보; 진성호; 안기용
- 발행일
- 2018-08
- 유형
- Article
- 저널명
- 콘크리트학회 논문집
- 권
- 30
- 호
- 4
- 페이지
- 383 ~ 390
- 언어
- KOR
- 출판사
- 한국콘크리트학회
- 발행국가
- 대한민국
- 분량
- 8 페이지
- ISSN
- E 2234-2842
P 1229-5515