CLASSIFICATION OF ALKALI ACTIVATED SLAG MORTAR ACCORDING TO MOST SUITABLE ACTIVATOR USAGE

초록

This paper deals with the replacement of OPC by ground granulated blast furnace slag (GGBS), activated with KOH, Ca(OH)2, NaOH at different concentrations.The main goal is to classify according to the type and activator content, what is the best usage for each kind of mortar, focusing on its practical applications. The development of compressive strength was measured at 7,14, 28, 56 and 91 days.Concerning workability, setting time was measured by needles penetration resistance immediately after casting of mortar. The pore structure of cement-free mortar was examined by the mercury intrusion porosimetry (MIP). In general, activated GGBS could achieve better results than OPC cement.For example,possibly improved durability in aggressive environments since the results about porosity showed more refinement, and also low heat of hydration. Also, following the results it was observed that the activator Ca(OH)2 is the most versatile even though it has limited compressive strength, around 13MPa at 3.0% concentration.Since for mortars this is not the only important characteristic to be analyzed, is important that it remains workable about 4 times more than OPC, what is important for some mortar usages.

제목
CLASSIFICATION OF ALKALI ACTIVATED SLAG MORTAR ACCORDING TO MOST SUITABLE ACTIVATOR USAGE
저자
안기용
발행일
2016-11-02