A novel method of fabricating ZnO/diamond/Si multilayers for surface acoustic wave (SAW) device applications

Citations

WEB OF SCIENCE

63
Citations

SCOPUS

67

초록

A novel process for fabricating ZnO/diamond/Si for a surface acoustic wave device is as follows: to form a trench of 10 mum in depth, the Si wafer is chemically etched by employing the SiO2 layer as a mask. Selective growth of polycrystalline diamond film is carried out by a microwave plasma CVD using nominal conditions of 700 W microwave power, 40 torr pressure, 0.5% CH4/H-2 ratio, 630 degreesC temperature, and -200 V bias enhancement for initial nucleation. After removing the SiO2 layer, indirect bonding of a Si handle wafer is performed at low temperatures of approximately 90 T. Finally, the bottom Si wafer is mechano-chemically polished until the surface (backside) of the diamond is exposed. Raman and field emission SEM observations show that a high quality diamond film is selectively grown only on the trenched Si region. It has also been found from the AFM results that the backside surface roughness of the exposed diamond film is measured to be lower than 10 nm. (C) 2002 Elsevier Science B.V. All rights reserved.

키워드

diamond; surface roughness; multilayers; plasma processing and deposition; SELECTIVE DEPOSITION; DIAMOND
제목
A novel method of fabricating ZnO/diamond/Si multilayers for surface acoustic wave (SAW) device applications
저자
Seo, Soo hyung; Shin, Wan chul; Park, Jin seok
DOI
10.1016/S0040-6090(02)00725-3
발행일
2002-09
유형
Article
저널명
Thin Solid Films
권
416
호
1-2
페이지
190 ~ 196